TM 5-826-6/AFR 93-5
Figure A-79. Medium severity transverse crock, case 2.
(c) High severity level (H). One of three conditions exists:
- Filled or nonfilled crack severity spalled with loose and missing particles (definite FOD potential) (figs.
A-80 through A-82).
- Nonfilled cracks with mean width greater than 1-inch creating tire damage potential.
- The slab is divided into 3 pieces by two or more cracks, or one or more of which is medium severity.
Figure A-80. High severity transverse crack.
A-46