Chapter 1. Introduction - ufc_3_260_16fa0010
Chapter 2. Basic Airfield Information
Chapter 3. Outline Of Basic Condition Rating Procedure
Distribution Of Condition Survey Reports.
Distribution of Condition Survey Reports cont. - ufc_3_260_16fa0016
Distribution of Condition Survey Reports cont. - ufc_3_260_16fa0017
Chapter 4. Sampling Techniques
Figure 4-1. Selection Of Minimum Number of Sample Units .
Figure 4-3. Example Division of Flexible pavement Feature Into Dample units
Chapter 5. Detailed Survey Procedure for Rigid Pavement
Figure 5-1. Jointed Pavements, Example Condition Survey Data Sheet.
Figure 5-2. Rigid Pavement Deduct Values, Distress 61, Blowup.
Figure 5-3. Rigid Pavement Deduct Values, Distress 62 Corner Break.
Figure 5-4. Rigid Pavement Deduct Values, Distress 63, Longitudinal/ Transverse/ diagonal cracking.
Figure 5-5. Rigid pavement deduct values, distress 64 durability cracking.
Figure 5-7. Rigid Pavement deduct Values, Distress 66 Patch.
Figure 5-8. Rigid Pavement Deduct Values , Distress 67, Patching. Utility Cut Defect
Figure 5-9. Rigid Pavement Deduct Values Distress 68 Popouts.
Figure 5-10. Rigid Pavement Deduct Values, Distress 69 Pumping
Figure 5-11. Rigid Pavement Deduct Values, Distress 70 Scaling .
Figure 5-12. Rigid Pavement Deduct Values, Distress 71, Settlement .
Figure 5-13. Rigid Pavement Deduct Values, Distress 72, Shattered Slab.
Figure 5-14. Rigid Pavement Deduct Values, Distress 7R Shrinkage Cracks .
Figure 5-15. Rigid Pavement Deduct Values, Distress 74, Spalling Along the Joints.
Figure 5-16. Rigid Pavement Deduct Values , Distress 75, Spalling Corner.
Figure 5-17. Corrected Deduct Values For Jointed Rigid Pavements.
Figure 5-18. Airfield PCI And Rating
Figure 5-19. Feature Summary, Jointed Rigid Pavement.
Chapter 6. Detailed Procedure for Flexible Pavement
Figure 6-1. Flexible Pavements, Example Condition Survey Data Sheet.
Figure 6-2. Flexible Pavement Deduct Values, Distress, 41, Alligator Cracking
Figure 6-3. Flexible Pavement Deduct Values, Distress 42, Bleeding
Figure 6-4. Flexible Pavement Deduct Values, Distress 43 Block Cracking.
Figure 6-5. Flexible Pavement Deduct Values, Distress 44, Corrugation.
Figure 6-6. Pavement Deduct Values, Distress 45, Depression.
Figure 6-7. Flexible Pavement Deduct Values, Distress 46, Jet Blast Erosion
Figure 6-8. Flexible Pavement Deduct Values, Distress 47, Joint Reflective Cracking.
Figure 6-9. Flexible Pavement Deduct Values, Distress 48, Longitudinal And Transverse Cracking .
Figure 6-10. Flexible Pavement Deduct Values, Distress 40, Oil Spillage.
Figure 6-11. Flexible Pavement Deduct Values, Distress 50, Patching And Utility Cut.
Figure 6-12. Flexible Pavement Deduct Values, Distress 51, Polished Aggregate.
Figure 6-13. Flexible Pavement Deduct Values, Distress 52, Raceling/ Weathering.
Figure 6-14. Flexible Pavement Deduct Values, Distress 53, Rutting.
Figure 6-15. Flexible Pavement Deduct Values, Distress 54, Shoving of Flexible Pavement by PCC Slabs
Figure 6-16. Flexible Pavement Educt Values, Distress 55, Slippage Cracking.
Figure 6-17. Flexible Pavement Deduct Values, Distress 56, Swell.
Figure 618. Corrected Deduct Values for Flexible Pavements
Figure 6-19. Features Summary for Flexible Pavements
Appendix A. Airfield Pavement Distress Identification
Table A. Frequently Occuring Identification Problems In Pavement Distress Identification
Table A. Frequently Occuring Identification Problems In Pavement Distress Identification - Continued
Table A-2. Summary of distress types and identification numbers
Figure A-1. Low severity alligator cracking, case 1.
Figure A-3. Low severity alligator cracking, approaching medium severity.
Measuring procedure.
Block cracking, distress 43.
Figure A-8. Low Severity Block Cracking, Case 1.
Figure A-10. Low severity Block Cracking Case 3.
Figure A-12. Medium Severity Block Cracking Case 2.
Figure A-14. Hogh Severity Block Cracking Case 2.
Measuring procedure.
Figure A-17. Low Severity Depression
Figure A-19. Medium Severity Depression case 2.
Figure A-21. Jet Blast Erosion, Case 1
Severity levels. - ufc_3_260_16fa0078
Figure A-24. Medium Seventy Joint reflection Cracking Case1.
Measuring procedure
Figure A-27. Low Seventy Longitudinal Crack.
Figure A-29. LOw Severity Crack, Porous Friction Course Pavement.
Figure A-31. Medium Severity Longitudinal Crack, Case 2.
Figure A-33. High Severity Longitudinal Crack.
Figure A-35. Oil Spillage, Case 1.
Figure A-37. Low Severity Patch, Case 1.
Figure A-39. Medium Severity Patch.
Raveling and weathering, distress 52.
Figure A-42. Low Severity Raveling/Weathering, Case 1.
Figure A-44. Typical Porous Friction Course Surface With no Raveling And Weathering , Case 1.
Figure A-46. Low Severity Raveling/ Weathering in Porous Friction Course Pavement.
Figure A-48. Medium Severity Raveling/ Weathering in Porous Friction course Pavement.
Figure A-50. High Severity Raveling/ Weathering .
Figure A-52. Low Severity Rutting.
Figure A-55. Medium severity rutting.
Shoving of asphalt pavement by PCC slabs, distress 54.
Slippage cracking, distress 55.
Severity levels. - ufc_3_260_16fa0098
Figure A-65. High Severity Swell.
Figure 66. Low Severity Blowup
Corner break, distress 62.
Figure A-70. Low Severity Corner Break, case 2.
Figure A-72. Medium Severity Corner Break, case 2.
Figure A-74. Low severity longitudinal crack.
Figure A-75. Low Severity Filled Longitudinal Cracks.
Figure A-77. Medium Severity Longitudinal Crack.
Figure A-79. Medium Severity Transverse Crock, case 2.
Figure A-81. High Severity Longitudinal Crack, Case 1.
Figure A-83. LOw Severity D Cracking.
Figure A-84. Medium Severity D Cracking Case 1.
Figure A-86. High Severity D cracking.
Figure A 88. Medium Seventy Joint Seal Damage.
Figure A-89. High Severity Joint Seal Damage.
Figure A-91. Low Severity Small Patch, Case 1.
Figure 93. Medium Seventy Small Patch Case 1.
Figure A-95. High Severity Small Patch.
Figure A -97. Low Severity Patch, Case 2.
Figure A-99. Medium Severity Utility cut.
Pumping, distress 69.
Figure 103. Pumpung (Note Stained Pavenet)
Scaling, map cracking, and crazing, distress 70.
Figure A. 108. Medium Severity Scalling
Figure A-109. High Severity Scalling
Figure A-111. Low severity settlement on apron, case 1.
Figure A-113. Medium severity settlement on apron.
Figure A-115. High severity settlement, case 2
Figure A-117. Low severity intersecting cracks, case 1.
Figure A-119. Medium severity intersecting cracks, case 1.
Figure A-121. Shattered slab.
Figure A-123. Shrinkage crack, case 2
Figure A-124. Low severity joint spall- case 1
Figure A-126. Medium severity joint spay case 1.
Figure A-129. High Severity Joint Spay case 2.
Figure A-130. Low Severity Corner Spall case 1
Figure A-32. Medium Severity Corner Spay case 1.
Figure A-134. High severity corner spall
Figure A-135. Flexible pavement condition survey data sheet (sample format)
Figure A-136. Rigid pavement condition survey data sheet (sample format)