TM 5-813-8
Figure 9-1. Break-point chlorination curve.
A high carbon dioxide content in reverse osmosis
A degasification tower is used to obtain equilibrium with
product water contributes to corrosion. This is true,
atmospheric carbon dioxide.
Degasification should
particularly where acid is fed for scale control.
occur after remineralization. Boiler feed water or wash
water should be drawn off prior to corrosion control.
9-2